Questions tagged [eutectic]
Eutectics are mixtures of solid chemicals that liquify at temperatures lower than the melting point of their constituents.
12
questions
1
vote
0
answers
55
views
Alkali-rich lead glass with working range at room temperature
I understand that the glass transition temperature (above which it is considered a super-cooled liquid) is quite far below the liquidus of the corresponding crystalline mixture. In the paper, "...
3
votes
3
answers
99
views
Eutectic temperatures of multicomponent metal carbides
Some carbides do not melt at atmospheric pressure. At high enough temperature, metallic element is in vapor phase. Experimentation with these systems is complicated because of their high melting or ...
0
votes
1
answer
50
views
Phase Diagram Vertical Lines
We had to create a phase diagram of H2O and NaCl. My professor mentioned that the vertical line I’ve encircled is at the weight % of 61.9. I was just wondering if this is proven through experiment or ...
2
votes
0
answers
109
views
Eutectic plot - freezing point lowering
I have a doubt about the correlation between eutectic plots and freezing point lowering.
The freezing point lowering, as well as all colligative properties, is defined in the presence of a volatile ...
3
votes
1
answer
534
views
Doesn't the eutectic diagram violate Gibbs's phase rule?
EDIT: As the question hasn't attracted any answers, I tried to put in more detail.
Gibbs's phase rule for a 2 component system at constant pressure says that $F=3-P$, i.e., that the number of degrees ...
0
votes
1
answer
272
views
Low temperature sodium salt eutectic [duplicate]
I have a need for a sodium salt that melts below 265 degrees celsius, which will be exposed to liquid sodium metal. The anion is not important, only that it has a sodium cation. I have done a lot of ...
0
votes
0
answers
3k
views
Eutectic Phase Diagram of Al-Si Analysis
Hello,
How can I know from this phase diagram:
1. The composition of the alloy Al-Si that allows precipitation to occure?
2. The range of temperatures where the Al-Si is soluble?
3. The range of ...
0
votes
0
answers
119
views
Literature values for NaCl Eutectic - Calculating the eutectic
For the NaCl eutectic I've seen two values widely used:
23.3wt% NaCl - James G. Speight: Lange's Handbook of Chemistry 2017)
5.1 M NaCl (Marion + Kargel 2008 - Cold Aqueous Planetary Geochemistry ...
1
vote
1
answer
626
views
How can I find the eutectic point of gallium and aluminum?
I've been interested in liquid metals for a while, but I've stayed away from mercury for obvious health reasons. I have a sample of gallium and I've seen a liquid metal mixture of gallium and aluminum....
2
votes
1
answer
2k
views
Melting point of ocean salt: eutectic?
I'm interested in the melting point of ocean salt. While sodium chloride has a melting point of 801 °C, ocean salt contains 15 % other ions, mainly sulphate, magnesium, calcium and potassium (the ...
2
votes
0
answers
177
views
What are the advantages of eutectic solvents over aqueous solutions for electroplating?
I'm trying to electrically strip lead contamination from aluminum.
This answer suggests using a deep eutectic solvent (DES) as the conducting liquid for plating the lead onto a copper cathode. But ...
4
votes
1
answer
636
views
Why did my deep eutectic solvent solidify?
I'm finally getting around to beginning to test this deep eutectic electrolyte. I mixed choline chloride with urea in a 1:2 mole ratio in a glass container. It formed a sludge. I sealed the ...