In this paper on page 1985 they say:
Fluorescence analysis confirmed that enhanced protein binding at higher electron dose depends only to a small extent on the slight increase in the lateral dimensions of the nanodeposits but to a much larger degree on their height (Figure 4E)
The amount of adsorbed IgG-Cy3 is largely independent of the actual area of the nominal 100 nm islands but scales with the height of the nanodeposits.
I don't understand this yet: why do I see that the fluorescence is proportional to area in this figure?