High-temperature interactions with salts on nichrome wire
I'm working on creating aluminium-doped zinc oxide (AZO) thin films, but instead of the usual glass substrate, I want to try this on a fine nichrome wire.
I'm using a mix of zinc acetate $\ce{Zn(...
4
votes
1
answer
99
views
Which reaction occurs in calcium vanadate when it comes in contact with water?
I am a physics student currently studying the electrical properties of $\ce{CaVO3}$ and I have noticed that the surface of my thin film samples, which were originally smooth and transparent, now have ...
1
vote
0
answers
136
views
How do I anodize bronze for thin film colors using electrolysis?
I am trying to change the color of the coins we have in Europe. I want to create patterns of certain colors.
They are made from "nordic gold" (89% copper, 5% aluminum, 5% zinc, and 1% tin).
...
1
vote
0
answers
45
views
“Good” properties of transparent conducting oxides
I'm a computer scientist and I'm trying to figure out which are the key properties that define a “good” acting transparent conducting oxide (TCO) in order to consider several possible features to ...
0
votes
0
answers
24
views
Copper Thin Film Oxidation?
So I am a clueless undergraduate student trying to get a glass substrate sputtered with a 100 to 200 nanometer copper thin film from one lab to another. I need to know how much time I have before the ...
4
votes
2
answers
351
views
How can I prevent my spin-coated silica thin film from cracking when I heat it up?
I am spin-coating a porous silica solution on a glass microscope coverslip, and then heating the resulting thin film to $\pu{350 °C}$, in an attempt to create a thin film of porous silica sol gel. I ...
1
vote
0
answers
24
views
AFM of Smooth Amorphous Carbon
I have been having trouble getting decent resolution images and clear data of smooth amorphous carbon thin films prepared by RF bias assisted vacuum deposition. I was using a DLC tip in tapping mode ...