All Questions
Tagged with iron oxidation-state
1
question with no upvoted or accepted answers
2
votes
0
answers
37
views
Is there any method to make sure a electroplated layer of iron oxidizes into magnetite (Fe3O4) instead of hematite (Fe2O3)?
I am currently electroplating iron on copper using a DIY setup in my lab. Steel sheet as anode with electrolyte having 5% acetic acid with sodium carbonate to form sodium acetate and added some NaCl ...