Which is a better poison to the Haber's process, $\ce{CO}$ or $\ce{H2S}$? [closed]
I am studying about catalysts and their promoters and poisons and came across two of the possible poisons for Fe used during Haber's process and wanted to compare their effect on the rates of reaction....
3
votes
0
answers
442
views
How to get rid of iron phosphate coating on steel after rust convertion
I tried to get rid of some mild rust on a couple of steel elements (cases, screws and whatnot). My intention was to get rid of physical rust by manually scraping it off, perhaps sandblasting and then, ...
0
votes
2
answers
246
views
How heating of iron results in formation of new compound? [closed]
Question:
Which of the following processes results in the formation of the new compound?
A. Dissolving common salt in water
B. Heating water
C. Heating of the platinum rod
D. Heating iron rod
I'...
-7
votes
1
answer
194
views
Can someone explain this answer in detail? [closed]
The density of iron is $\pu{7.874 g/cm3}$ and its unit cell volume is $\pu{2.364E-23 cm3}$. These values indicate that there are: two Fe atoms per unit cell and the metal is body-centered cubic.
I am ...
1
vote
0
answers
798
views
How to prepare a solution of Ferrous Iron?