7 votes
1 answer
6k views

Creating resilient (non-brittle non-water-soluble) verdigris (blue-green copper patina)

First off, I checked and there are indeed a number of questions on copper patinas, but none which deal with resilience. Context I own a number of copper writing utensils, which I'd like to get a nice ...
TheChymera's user avatar
3 votes
1 answer
240 views

Nichrome alloy corrosion at high temperature

We are currently using a nichrome (80/20) wire based heater to surround a sample chamber that we wish to heat by radiation. Maximum sample temperature is 400degC in an atmosphere of air that may be ...
Dirk Bruere's user avatar
  • 1,672
0 votes
1 answer
174 views

Why is nickel anticorrosive?

I've been looking into corrosion and common ways to prevent it. Pure nickel seems to be the main anticorrosive material to use, but I can't find a decent answer as to what it has/does that other ...
cass's user avatar
  • 1
3 votes
0 answers
85 views

Is hydrochloric acid or sulfuric acid more corrosive to titanium?

Which acid is more corrosive to titanium at 20 to 30 °C and similar concentrations: hydrochloric acid $\ce{HCl}$ or sulfuric acid $\ce{H2SO4}$? I found some info on AZoMaterials — Titanium - Corrosion ...