Will strong base corrode aluminium in absence of oxygen? [closed]
From what i understand, putting iron in a vacuum chamber (airtight container) will stops further oxidation take place.
However in aluminium, with only oxygen, aluminium will form thin oxide film that ...
9
votes
1
answer
850
views
What happens to the carbon in carbon steel when it rusts?
Carbon steel is iron containing some carbon in various forms of iron carbide.
When it rusts (oxidises), the iron becomes part of all kinds of crystalline and amorphous iron oxides and hydroxides, ...